Which fibre to resin (%) ratio for advanced composite wet lay-ups is generally considered the best?

  • 60:40.
  • 50:50.
  • 40:60.

Explanation from PART66Online

For advanced-composite wet lay-ups the generally preferred fibre-to-resin ratio is about 60:40 by volume; this gives enough fibre to carry load while leaving just enough resin to wet out and bond the fibres. Too much resin (50:50 or 40:60) adds weight and lowers strength without benefit.

A

azwanmaziz92 asked · 5 Sep 2013

Referring to Jeppesen Airframe book. It states that ratio is 60% fibre and 40% resin.. please explain

Community Comments (1)

P
PART66Online 5 Sep 2013
Hello.

Could you please send that book to info@part66online.com ? I can send you some other books for modules if you need.

Please Sign In to post a comment.

We use essential cookies to keep you signed in, plus anonymous analytics to understand how the site is used. Cookie-based analytics is set only with your consent. See our Privacy & Cookie Policy.